Abstract
Many shearing, blanking, and piercing operations are based on the same underlying principles of shear mechanisms. This article provides information on the various operations associated with die cutting and describes three phases involved in the shear cutting or punching action. These phases include deformation, penetration and fracture. The article also explains the effect of clearance on tool life and force and power requirements. It reviews the forces involved in the punching process and describes the diameter of a hole or blank in relation to material thickness. The limitations of punching are also discussed. The article describes the relationship of the die clearance to stress-strain curves and explains the procedure of interpreting the stress-strain curves. The article concludes with information on the dynamic stripping forces in blanking.
Principles of Shearing, Blanking, and Piercing, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 28–38, https://doi.org/10.31399/asm.hb.v14b.a0005116
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!