Forming of Nickel and Cobalt Sheet Alloys[1]
Revising author
-
Published:2006
Abstract
This article tabulates the nominal compositions for nickel and cobalt alloys. It illustrates the comparison of strain-hardening rates of a number of alloys in terms of the increase in hardness with increasing cold reduction. The forming practice for age-hardenable alloys and the lubricants used in the forming processes of nickel and cobalt alloys are also discussed. The article summarizes the modification of tools and dies used for cold forming other metals, as the physical and mechanical properties of nickel and cobalt alloys frequently necessitate it. It discusses forming techniques for these alloys and provides several examples of these techniques, which include shearing, blanking, piercing, deep drawing, spinning, explosive forming, bending, and expanding/tube forming.
Howard W. Sizek, Forming of Nickel and Cobalt Sheet Alloys, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 640–651, https://doi.org/10.31399/asm.hb.v14b.a0005145
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.