Shearing of Sheet, Strip, and Plate
Revising author
-
Published:2006
Abstract
Shearing is a method for cutting a material piece into smaller pieces using a shear knife to force the material past an opposition shear knife in a progression form. This article describes the principles, attributes, and defects of straight-knife shearing. The equipment, materials used, and the operating parameters are discussed. The article provides information on the applications of rotary shearing. It concludes with a discussion on devices equipped with shearing machines for protecting personnel from the hazards of shear knives, flywheels, gears, and other moving parts.
L. Chen, Shearing of Sheet, Strip, and Plate, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 39–45, https://doi.org/10.31399/asm.hb.v14b.a0005102