Abstract
This article summarizes the metallurgical and environmental variables that affect fracture toughness, fatigue life, and subcritical crack growth of titanium alloys, such as chemistry, microstructure, texture, environment, and loading. The classes of titanium alloys considered in the article include alpha-beta alloys, Ti-6AI-4V; alpha alloys, Ti-8Al -1Mo-IV, Ti-5AI-2.5Sn, Ti-6242S; and beta alloys, solute-lean beta alloys and solute-rich beta alloys.
Fatigue and Fracture Properties of Titanium Alloys, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 829–853, https://doi.org/10.31399/asm.hb.v19.a0002409