Abstract
This article focuses on the subject of proactive or predictive maintenance with particular emphasis on the control and prediction of corrosion damage for life extension and failure prevention. It discusses creep life assessment from the perspective of creep-rupture properties and creepcrack growth. Practical methods based on replication and parametric approaches are also discussed.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
P.F. Timmins, Failure Control in Process Operations, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 468–482, https://doi.org/10.31399/asm.hb.v19.a0002387
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Glossary of Terms—Failure Analysis and Prevention
Failure Analysis and Prevention (2021 Edition)
Glossary: Failure Analysis and Prevention
Failure Analysis and Prevention
Elevated-Temperature Crack Growth
Fatigue and Fracture
Gallery of Corrosion Damage
Corrosion: Materials
Corrosion Monitoring Using Microwave and Guided Wave Nondestructive Evaluation
Corrosion: Fundamentals, Testing, and Protection
What Is a Failure?
How to Organize and Run a Failure Investigation
Materials Selection for Failure Prevention
Failure Analysis and Prevention
Materials Selection for Failure Prevention
Analysis and Prevention of Component and Equipment Failures
Reliability-Centered Maintenance
Analysis and Prevention of Component and Equipment Failures
Glossary of Terms—Analysis and Prevention of Component and Equipment Failures
Analysis and Prevention of Component and Equipment Failures