Hot Working Simulation by Hot Torsion Testing[1]
By
Joseph R. Pickens
Joseph R. Pickens
Concurrent Technologies Corporation
Search for other works by this author on:
-
Published:2005
Publication history
March 09, 2009
Abstract
This article summarizes the types of hot working simulation tests such as hot tension, compression, and torsion testing used in the assessment of workability. It illustrates the use of hot torsion testing for the optimization of hot working processes. The article concludes with information on some hot torsion application examples.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Joseph R. Pickens, Hot Working Simulation by Hot Torsion Testing, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, https://doi.org/10.31399/asm.hb.v14a.a0009012
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Torsion Testing to Assess Bulk Workability
Metalworking: Bulk Forming
Mechanical Behavior
Fatigue and Fracture Understanding the Basics
Hot Tension and Compression Testing
Mechanical Testing and Evaluation
Hot-Tension Testing
Metalworking: Bulk Forming
Useful Formulas for Deformation Analysis and Workability Testing
Metalworking: Sheet Forming
Stress Relaxation Testing
Mechanical Testing and Evaluation
Recovery Hopkinson Bar Techniques
Mechanical Testing and Evaluation
Mechanical Testing
Metals Handbook Desk Edition (2nd Edition)
Mechanical Behavior
Elements of Metallurgy and Engineering Alloys
Useful Formulas for Metals Processing
Metals Process Simulation