Metalworking: Bulk Forming
Flat, Bar, and Shape Rolling
-
Published:2005
Abstract
The primary objectives of the rolling process are to reduce the cross section of the incoming material while improving its properties and to obtain the desired section at the exit from the rolls. This article illustrates a rolling sequence for the fabrication of bars, shapes, and flat products from blooms, billets, and slabs. It describes two methods for shapes or sections: universal rolling and caliber rolling. The article provides information on two-high mills and three-high mills. Specialty mills for thin sheets, namely, the Sendzimir mill and planetary mill, are discussed. The article analyzes the components of a computer controlled...
Sign in
ASM members
Member Sign InG.D. Lahoti, P.M. Pauskar, Flat, Bar, and Shape Rolling, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 459–479, https://doi.org/10.31399/asm.hb.v14a.a0004009
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field