Forging of Carbon and Alloy Steels
-
Published:2005
Abstract
This article focuses on the forging behavior and practices of carbon and alloy steels. It presents general guidelines for forging in terms of practices, steel selection, forgeability and mechanical properties, heat treatments of steel forgings, die design features, and machining. The article discusses the effect of forging on final component properties and presents special considerations for the design of hot upset forgings.
C.J. Van Tyne, Forging of Carbon and Alloy Steels, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 241–260, https://doi.org/10.31399/asm.hb.v14a.a0003991