Abstract
For forming processes, optimization goals range from tuning the process parameters while keeping geometry unchanged to finding optimal geometry for intermediate dies in a multistage forming operation. This article commences with a description on the three salient steps of optimization procedures: defining the objective function, calculating the objective function, and searching an optimum design. It concludes with an example illustrating the optimization of conical-die extrusion.
You do not currently have access to this chapter.
Citation
Anil Chaudhary, Suhas Vaze, Design Optimization for Dies and Preforms, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 640–644, https://doi.org/10.31399/asm.hb.v14a.a0004022
Download citation file:
Related Book Content
Forming of Beryllium
Metalworking: Sheet Forming
Useful Formulas for Deformation Analysis and Workability Testing
Metalworking: Bulk Forming
Forming of Titanium Plate, Sheet, Strip, and Tubing
Titanium Physical Metallurgy, Processing, and Applications
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Forging and Forming
Superalloys: A Technical Guide (Second Edition)
Casting, Forming, and Forging
Gear Materials, Properties, and Manufacture
Introduction
Tool Steels (Fifth Edition)
Design Guidelines for Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
Wrought Aluminum Processes and Products
Aluminum Science and Technology
Powder Hot Pressing and Forging
Powder Metallurgy