Failure Analysis and Prevention
Failure Assessment Diagrams
-
Published:2002
Abstract
Optimized modeling of fracture-critical structural components and connections requires the application of elastic-plastic fracture mechanics. Such applications, however, can require sophisticated analytical techniques such as crack tip opening displacement (CTOD), failure assessment diagram (FAD), and deformation plasticity failure assessment diagram (DPFAD). This article presents the origin and description of FAD and addresses R6 FAD using J-integral. It details the fracture criteria of BS 7910. The factors to be considered during the use of FAD and the applications of FAD are also reviewed.
Harold S. Reemsnyder, Failure Assessment Diagrams, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 243–249, https://doi.org/10.31399/asm.hb.v11.a0003513
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.