Failures of Lifting Equipment[1]
By
Frank L. Jamieson
Frank L. Jamieson
Stelco Inc.
retired
Search for other works by this author on:
-
Published:2002
Abstract
This article focuses on the mechanisms and common causes of failure of metal components in lifting equipment in the following three categories: cranes and bridges, particularly those for outdoor and other low-temperature service; attachments used for direct lifting, such as hooks, chains, wire rope, slings, beams, bales, and trunnions; and built-in members such as shafts, gears, and drums.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Frank L. Jamieson, Failures of Lifting Equipment, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, https://doi.org/10.31399/asm.hb.v11.a0001811
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Failures of Cranes and Lifting Equipment
Analysis and Prevention of Component and Equipment Failures
Brittle Failure of a Hook Initiated at a Pre-existing Defect
ASM Failure Analysis Case Histories: Material Handling Equipment
Fatigue Fracture of a 1040 Steel Coil Hook
ASM Failure Analysis Case Histories: Material Handling Equipment
Fatigue Fracture of a 1020 Steel Crane Hook
ASM Failure Analysis Case Histories: Material Handling Equipment
Corrosion Fatigue Cracking of Wire Ropes
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Brittle Rupture of a Chain Sling
ASM Failure Analysis Case Histories: Material Handling Equipment
Fatigue Failures of Links from Grab Chains
ASM Failure Analysis Case Histories: Material Handling Equipment
Brittle Fracture of a Crane Hook
ASM Failure Analysis Case Histories: Material Handling Equipment
The Influence of Wear on the Fatigue Failure of a Wire Rope
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Failure of Some Electrically Butt-Welded Mild-Steel Chains
ASM Failure Analysis Case Histories: Material Handling Equipment