Corrosive Wear Failures
-
Published:2002
Abstract
This article focuses on the corrosion-wear synergism in aqueous slurry and grinding environments. It describes the effects of environmental factors on corrosive wear and provides information on the impact and three-body abrasive-corrosive wear. The article also discusses the various means for combating corrosive wear, namely, materials selection, surface treatments, and handling-environment modifications.
You do not currently have access to this chapter.
Citation
Corrosive Wear Failures, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, p 989–994, https://doi.org/10.31399/asm.hb.v11.a0003567
Download citation file:
Related Book Content
Tribocorrosion
Friction, Lubrication, and Wear Technology
Corrosive Wear Failures
Failure Analysis and Prevention (2021 Edition)
Impact Wear Failures
Failure Analysis and Prevention (2021 Edition)
Impact Wear
Friction, Lubrication, and Wear Technology
Introduction to Selection of Titanium Alloys
Titanium: A Technical Guide (Second Edition)
Performance of Refractories in Severe Environments
Corrosion: Materials
Wear Testing
Metals Handbook Desk Edition (2nd Edition)
Glossary of Terms
Surface Engineering for Corrosion and Wear Resistance
Selection Guidelines for Lightweight Materials
Lightweight Materials Understanding the Basics
Some Considerations in the Selection of a Superalloy
Superalloys Alloying and Performance