Book Chapter
Weldability of Ferrous and Nonferrous Alloys
-
Published:2011
Abstract
Weldability refers to the ease of welding a material under the imposed fabrication conditions to perform satisfactorily during service. This article is a comprehensive collection of tables that summarize the general weldability of cast irons, steels, nonferrous metals, and their alloys by common fusion welding processes.
You do not currently have access to this chapter.
Citation
Weldability of Ferrous and Nonferrous Alloys, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 874–877, https://doi.org/10.31399/asm.hb.v06a.a0005644
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Metallurgy Variables in Fusion Welding
Joining Understanding the Basics
Reference Tables
Weld Integrity and Performance
Glossary of Terms: Surface Engineering
Surface Engineering
Energy Sources Used for Fusion Welding
Welding, Brazing, and Soldering
Selection of Wrought Duplex Stainless Steels
Welding, Brazing, and Soldering
Welding Process Fundamentals
Welding Fundamentals and Processes
Tin Plating
Surface Engineering
Introduction to Integrated Weld Modeling
Metals Process Simulation
Metallography and Microstructures of Ductile Irons
Cast Iron Science and Technology
Origin of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels