Welding Fundamentals and Processes
Summary of Fusion Welding Processes
-
Published:2011
Abstract
This article is a compilation of tables summarizing the fusion welding process. Included in the article is a table that presents the various fusion welding and cutting processes and their applications. Information on the general characteristics of arc welding processes is tabulated. The article also contains a list of the various criteria for selecting the suitable welding process for carbon steels.
Summary of Fusion Welding Processes, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 870–873, https://doi.org/10.31399/asm.hb.v06a.a0005643