Residual Stresses and Distortion[1]
By
Koichi Masubuchi
Koichi Masubuchi
Massachusetts Institute of Technology
Search for other works by this author on:
-
Published:2011
Abstract
This article describes the formation of residual stresses and distortion and the techniques for measuring residual stresses. It provides a discussion on the magnitude and distribution analysis of residual stresses and distortion in weldments. The article considers the effects of residual stresses and distortion on the brittle fracture and fatigue fracture of welded structures. The thermal treatments of weldments are also discussed.
You do not currently have access to this chapter.
Citation
Koichi Masubuchi, Residual Stresses and Distortion, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 158–168, https://doi.org/10.31399/asm.hb.v06a.a0005617
Download citation file:
Related Book Content
Residual Stresses and Distortion
Welding, Brazing, and Soldering
Introduction to Integrated Weld Modeling
Metals Process Simulation
Fitness-for-Service Assessment of Welded Structures
Welding, Brazing, and Soldering
Heat Flow in Fusion Welding
Welding Fundamentals and Processes
Numerical Aspects of Modeling Welds
Welding, Brazing, and Soldering
Basic Understanding of Weld Corrosion
Corrosion of Weldments
Corrosion of Weldments
Welding, Brazing, and Soldering
Properties of Carbon Alloy Steel Welds
Weld Integrity and Performance
Failure and Stress Analysis of Deformed Steel Tube
Handbook of Case Histories in Failure Analysis
Corrosion of Ferritic Stainless Steel Weldments
Corrosion of Weldments