White Iron and High-Alloyed Iron Castings
-
Published:2008
Abstract
This article presents a discussion on the melting, pouring, and shakeout practices; composition control; molds, patterns, and casting design; heat treatment; and applications of different classes of nickel-chromium white irons and high-chromium white irons.
Sign in
ASM members
Member Sign InRichard B. Gundlach, White Iron and High-Alloyed Iron Castings, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 896–903, https://doi.org/10.31399/asm.hb.v15.a0005327