Abstract
The cold chamber die casting process is used with higher-melting-point alloys such as aluminum and magnesium. This article discusses the component design of the cold chamber high-pressure die casting machine. It reviews the process parameters of cold chamber die casting, incuding the shot profile, intensification phase, and component size.
Robert J. McInerney, II, Cold Chamber Die Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 724–726, https://doi.org/10.31399/asm.hb.v15.a0005268