Corrosion of Metal Processing Equipment
Revising author
-
Published:2006
Abstract
The high-temperature corrosion processes that are most frequently responsible for the degradation of furnace accessories are oxidation, carburization, decarburization, sulfidation, molten-salt corrosion, and molten-metal corrosion. This article discusses each corrosion process, along with the corrosion behavior of important engineering alloys. It describes the corrosion of plating, anodizing, and parts of pickling equipment such as tanks, wirings and bus bars, racks, anode splines, pumps, and heaters.
B. Mishra, Corrosion of Metal Processing Equipment, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 1067–1075, https://doi.org/10.31399/asm.hb.v13c.a0004218