Organic coatings are the principal means of corrosion control for the hulls and topsides of ships and for the splash zones on permanent offshore structures. This article describes surface preparation which is the most important consideration in determining the performance of organic coating systems. It contains a table that lists the uses and applicable standards for various surface preparation techniques. The article provides information on organic coatings in topside coating systems and reviews the importance of primers in the protection of steel substrates. It also explains the property requirements and the common types of immersion coatings.
R.D. Granata, Performance of Organic Coatings, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 69–72, https://doi.org/10.31399/asm.hb.v13c.a0004108
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.