Abstract
This article discusses the general properties of ocean water and their effects on corrosion. It describes the major and minor features of the ocean water on corrosion, including the effects of variability, pollutants, and fouling organisms. Effects of water flow velocity on marine corrosion are also reviewed.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Stephen C. Dexter, Corrosion in Seawater, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 27–41, https://doi.org/10.31399/asm.hb.v13c.a0004105
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Compatibility Guide
Corrosion: Materials
Corrosion of Metal Artifacts and Works of Art in Museum and Collection Environments
Corrosion: Environments and Industries
Corrosion of Metal Artifacts Displayed in Outdoor Environments
Corrosion: Environments and Industries
Aqueous Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
Statistical Aspects of Design
Materials Selection and Design
Glossary of Corrosion-Related Terms
Corrosion: Understanding the Basics
Global Cost of Corrosion—A Historical Review
Corrosion: Materials
Glossary of Terms
Corrosion in the Petrochemical Industry (Second Edition)
Introduction to Metallurgically Influenced Corrosion
Corrosion: Fundamentals, Testing, and Protection
Liquid Metal Corrosion and Embrittlement
High-Temperature Corrosion and Materials Applications