A close-interval survey (CIS) is a series of structure-to-electrolyte direct current potential measurements performed at regular intervals for assessing the level of cathodic protection (CP) on pipelines and other buried or submerged metallic structures. This article describes the equipment required to perform the CIS. It provides a discussion on the activities that should be performed during the preparation and execution of the CIS. The dynamic stray current identification and compensation by CIS is discussed briefly. The article also explains various factors involved in the validation of CIS data. It concludes with information on CIS data interpretation.
Sign in
ASM members
Member Sign InDrew Hevle, Angel Kowalski, Close-Interval Survey Techniques, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 84–88, https://doi.org/10.31399/asm.hb.v13c.a0004112
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.