Corrosion of Wrought Low-Alloy Steels
Revising author
-
Published:2005
Abstract
Low-alloy steels are used in a broad spectrum of applications. In some cases, corrosion resistance is a major factor in alloy selection; in other applications, it is only a minor consideration. This article reviews the applications of alloy steel products in four major industries, namely, oil and gas production, energy conversion systems, marine applications, and chemical processing. Emphasis is placed on the corrosion characteristics of the products, which are used in various applications of each industry.
Thomas G. Oakwood, Corrosion of Wrought Low-Alloy Steels, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 11–27, https://doi.org/10.31399/asm.hb.v13b.a0003806