Corrosion Rate Conversion
-
Published:2005
Abstract
This article contains a corrosion rate conversion table, and a figure, that illustrate relationships among some of the units commonly used for corrosion rates of metals.
Topics
Corrosion
You do not currently have access to this chapter.
Citation
Corrosion Rate Conversion, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 675, https://doi.org/10.31399/asm.hb.v13b.a0003794
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Corrosion Data
Titanium: A Technical Guide (Second Edition)
Corrosion Rate Conversion
Corrosion in the Petrochemical Industry (Second Edition)
Types of Corrosive Environments
Corrosion of Aluminum and Aluminum Alloys
Microbiologically Influenced Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Electrochemical Corrosion-Rate Measurements
Fundamentals of Electrochemical Corrosion
Methods for Measuring Gaseous Corrosion Rates
Corrosion: Fundamentals, Testing, and Protection
Potential Measurements with Reference Electrodes
Corrosion: Fundamentals, Testing, and Protection
Zinc-Rich Coatings
Protective Organic Coatings