Modeling and Simulation of Press and Sinter Powder Metallurgy[1]
-
Published:2015
Abstract
This article discusses continuum modeling, which is the most relevant approach in modeling grain growth, densification, and deformation during sintering. Continuum plasticity models are frequently used to describe the mechanical response of metal powders during compaction. The article illustrates the typical procedure for computer simulation for press and sinter process. It describes the procedure to obtain the material properties based on the generalized Shima-Oyane model. The article presents a wide variety of tests, accounting for data on the grain growth, densification, and distortion where these data help in the development of a constitutive model for sintering simulation. Finally, the...
Sign in
ASM members
Member Sign InSuk Hwan Chung, Young-Sam Kwon, Seong Jin Park, Randall M. German, Modeling and Simulation of Press and Sinter Powder Metallurgy, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 179–190, https://doi.org/10.31399/asm.hb.v07.a0006033
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.