Applications for Metal Powder Injection Molding
-
Published:2015
Abstract
Metal injection molding (MIM) is a metalworking technology that has its origins as a commercial technology only dating back to the early 1970s. This article explores why the MIM is the preferred solution for many fabricated components. It illustrates the MIM components required for different end-use markets such as electronics and telecommunications, medical, automotive, power hand tools, industries, and firearms.
Sign in
ASM members
Member Sign InMatt Bulger, Paul Hauck, Applications for Metal Powder Injection Molding, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 855–859, https://doi.org/10.31399/asm.hb.v07.a0006055