Compaction of Carbide Powders
By
Pankaj K. Mehrotra
Pankaj K. Mehrotra
Kennametal Inc.
Search for other works by this author on:
-
Published:2015
Abstract
Consolidation and shaping of grade powders is carried out using several methods, depending on the size, complexity, shape, and quantity of parts required. This article details the powder consolidation methods of carbide powders: uniaxial pressing, cold isostatic pressing, extrusion, green machining, and injection molding.
You do not currently have access to this chapter.
Citation
Neal Myers, Pankaj K. Mehrotra, Compaction of Carbide Powders, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 715–719, https://doi.org/10.31399/asm.hb.v07.a0006053
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Shaping Processes
Binder and Polymer Assisted Powder Processing
Pressing and Sintering of Titanium Powders
Powder Metallurgy
Design for Plastics Processing
Materials Selection and Design
Forming and Predensification of Ceramics
Engineered Materials Handbook Desk Edition
Beryllium and Aluminum-Beryllium Alloys
Powder Metallurgy
Modeling and Simulation of Press and Sinter Powder Metallurgy
Metals Process Simulation
Beryllium
Lightweight Materials Understanding the Basics
Research and Development
Aluminum Extrusion Technology
List of Formula Symbols
Extrusion (Second Edition)
Thermodynamics in Extrusion
Aluminum Extrusion Technology