Powder Hot Pressing and Forging[1]
By
Howard A. Kuhn
Howard A. Kuhn
Concurrent Technologies Corporation (CTC)
Revising author
Search for other works by this author on:
-
Published:2015
Publication history
August 22, 2015
Search within book:
Abstract
Successful application of forging and hot pressing involves careful consideration of powder preparation and forming process parameters. This article describes the important process features for powder forging and hot pressing, along with specific applications and materials used.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Howard A. Kuhn, Powder Hot Pressing and Forging, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 271–276, https://doi.org/10.31399/asm.hb.v07.a0006080
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Ferrous Powder Metallurgy Materials
Properties and Selection: Irons, Steels, and High-Performance Alloys
Powder-Forged Steel
Powder Metallurgy
Glossary of Terms: Modeling for Metals Processing
Fundamentals of Modeling for Metals Processing
Ceramic-Matrix Composites
Lightweight Materials Understanding the Basics
High-Density Ferrous Powder Metallurgy Parts
Metals Handbook Desk Edition (2nd Edition)
Process Modeling
Thermal Spray Technology
Probability of Detection
Nondestructive Evaluation of Materials
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Forming of Titanium Plate, Sheet, Strip, and Tubing
Titanium Physical Metallurgy, Processing, and Applications
Design for Powder Metallurgy
Materials Selection and Design