Tin Plating
By
Arthur J. Killmeyer
Arthur J. Killmeyer
Tin Information Center of North America
Revising author
Search for other works by this author on:
-
Published:1994
Abstract
A tin deposit provides sacrificial protection to copper, nickel, and many other nonferrous metals and alloys. Tin also provides good protection to steel. Tin can be deposited from either alkaline or acid electrolytes. This article explains the compositions and operating conditions of these electrolytes.
You do not currently have access to this chapter.
Citation
Arthur J. Killmeyer, Tin Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 239–241, https://doi.org/10.31399/asm.hb.v05.a0001250
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Glossary of Terms: Surface Engineering
Surface Engineering
Weldability of Ferrous and Nonferrous Alloys
Welding Fundamentals and Processes
Plating Adherence Problems in Electronic Components
ASM Failure Analysis Case Histories: Processing Errors and Defects
Bainitic Structures
Metallography and Microstructures
Massive Transformation Structures
Metallography and Microstructures
Nonferrous Metals
Elementary Materials Science
Periodic Table of Elements
Fundamentals of Modeling for Metals Processing
Retrogression and Reaging
Heat Treating of Nonferrous Alloys
Mössbauer Spectroscopy
Materials Characterization
Voltammetry
Materials Characterization