Abstract
The chemicals that have been used in traditional vapor degreasing have serious health and environmental hazards that have prompted the search for modified and alternative techniques. This article provides a detailed discussion on the regulatory mandates that affect the use of industrial degreasing methods. It describes the aqueous degreasing technique, which forms an attractive alternative to the traditional vapor degreasing process. The article includes information on the materials and equipment used in the process, and discusses the advantages and disadvantages of hot and dip tank systems of aqueous degreasing. It explains how to convert an existing vapor degreaser to...
Sign in
ASM members
Member Sign InDennis Zupan, Tony L. Green, Donald W. Benjamin, Bruce Hooke, Calvin Fong, Vapor Degreasing Alternatives, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 930–934, https://doi.org/10.31399/asm.hb.v05.a0001324
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!