This article provides an overview of plasma surface treatments for plastics. It covers the equipment and methods used in plasma processing, providing detailed explanations of the plasma discharge reactions and how they affect surface state and topography. It also provides information on contamination removal, plasma surface modification, plasma-induced grafting, and plasma film deposition.
Om S. Kolluri, Plasma Surface Engineering of Plastics, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 892–899, https://doi.org/10.31399/asm.hb.v05.a0001319