Multiple-Layer Alloy Plating
By
Daniel T. Schwartz
Daniel T. Schwartz
University of Washington
Search for other works by this author on:
-
Published:1994
Abstract
Multiple-layer alloy electrodeposition involves the formation of an inhomogeneous alloy consisting of lamellae of different composition. This article reviews the process description, engineering parameters, characterization, and applications of multiple-layer alloys. Pulsed-current plating and pulsed-potential plating are also discussed.
You do not currently have access to this chapter.
Citation
Daniel T. Schwartz, Multiple-Layer Alloy Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 274–276, https://doi.org/10.31399/asm.hb.v05.a0001260
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Plasma Carburizing
Steel Heat Treating Fundamentals and Processes
Pulsed-Current Plating
Surface Engineering
Continuous Electrodeposited Coatings for Steel Strip
Surface Engineering
Zinc Alloy Plating
Surface Engineering
Indium Plating
Surface Engineering
Smart Coatings and Nanotechnology Applications in Coatings
Protective Organic Coatings
Compliant Organic Coatings
Surface Engineering
Microstructural Characterization of Coatings and Thin Films
Surface Engineering
Electrodeposition Processes
Metals Handbook Desk Edition (2nd Edition)
Industrial (Hard) Chromium Plating
Surface Engineering