Abstract
This article explains the applications of continuous electroplated steel. For each category of application, the type of coating needed and the key attributes of the coating are discussed. The bulk of the article describes electrodeposition technology, including plating line components and process classification.
You do not currently have access to this chapter.
Citation
Stavros G. Fountoulakis, Continuous Electrodeposited Coatings for Steel Strip, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 349–359, https://doi.org/10.31399/asm.hb.v05.a0001271
Download citation file:
November 12-16 | Phoenix, Arizona
Keep up-to-date at the premier event for the microelectronics failure analysis community. Register today for ISTFA 2023!
Related Book Content
Dip, Barrier, and Chemical Conversion Coatings
Metals Handbook Desk Edition (2nd Edition)
Multiple-Layer Alloy Plating
Surface Engineering
Indium Plating
Surface Engineering
Smart Coatings and Nanotechnology Applications in Coatings
Protective Organic Coatings
Microstructural Characterization of Coatings and Thin Films
Surface Engineering
Compliant Organic Coatings
Surface Engineering
Electrodeposition Processes
Metals Handbook Desk Edition (2nd Edition)
Industrial (Hard) Chromium Plating
Surface Engineering
Chemical and Electrolytic Methods of Powder Production
Powder Metallurgy
Tin Alloy Plating
Surface Engineering