Abstract
This article provides information on the compositions of alkaline and acid baths and process parameters for zinc-iron, zinc-cobalt, zinc-nickel, and tin-zinc plating.
You do not currently have access to this chapter.
Citation
Nabil Zaki, Zinc Alloy Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 264–265, https://doi.org/10.31399/asm.hb.v05.a0001257
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Plasma Carburizing
Steel Heat Treating Fundamentals and Processes
Multiple-Layer Alloy Plating
Surface Engineering
Tin Alloy Plating
Surface Engineering
Glossary of Terms: Corrosion
Corrosion: Fundamentals, Testing, and Protection
Cold Spray Coating Applications in Protection and Manufacturing
High Pressure Cold Spray Principles and Applications
Introduction to Surface Engineering for Corrosion and Wear Resistance
Surface Engineering for Corrosion and Wear Resistance
Corrosion Control for Marine- and Land-Based Infrastructure Applications
Thermal Spray Technology
Introduction to Methods of Corrosion Protection
Corrosion: Fundamentals, Testing, and Protection
Waste-to-Energy Boilers and Waste Incinerators
High-Temperature Corrosion and Materials Applications
Wax-Based Coating Systems
Protective Organic Coatings