Surface Engineering
Tin Alloy Plating
-
Published:1994
Abstract
Electrodeposition of tin alloys is used to protect steel against corrosion or wear, to impart resistance to etching, and to facilitate soldering. This article focuses on the compositions, operating conditions, advantages, and limitations of methane sulfonic acid plating solutions and fluoborate plating solutions for tin-lead. It briefly describes the solution compositions and operating conditions of tin-bismuth, tin-nickel, and tin-zinc.
Reginald K. Asher, Sr., Tin Alloy Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 258–263, https://doi.org/10.31399/asm.hb.v05.a0001256