Abstract
Copper alloys are widely used as electroplated coatings. They can also be used with practically any substrate material that is suitable for electroplating. This article focuses on the solution composition and operating conditions for brass and bronze plating solutions. It describes the decorative and engineering applications of brass and bronze plating. The article also provides information on the treatment of waste water from brass and bronze plating operations.
Henry Strow, Copper Alloy Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 255–257, https://doi.org/10.31399/asm.hb.v05.a0001255