Online Monitoring and Control of Polymer Additive Manufacturing Processes
-
Published:2023
Abstract
Additive manufacturing (AM) is a revolutionary technology that fabricates parts layerwise and provides many advantages. This article discusses polymer AM processes such as material extrusion, vat photopolymerization (VPP), powder-bed fusion (PBF), binder jetting (BJ), material jetting (MJ), and sheet lamination (SL). It presents the benefits of online monitoring and process control for polymer AM. It also introduces the respective monitoring devices used, including the models and algorithms designed for polymer AM online monitoring and control.
Chaoran Dou, Daniel Elkins, Zhenyu (James) Kong, Chenang Liu, Online Monitoring and Control of Polymer Additive Manufacturing Processes, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 1–13, https://doi.org/10.31399/asm.hb.v24A.a0006968
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.