Weld Integrity and Performance
Chapter 11: Corrosion of Weldments[1]
-
Published:1997
Abstract
This article describes some of the general characteristics associated with the corrosion of weldments. The role of macrocompositional and microcompositional variations, a feature common to weldments, is emphasized in this article to bring out differences that need to be realized in comparing corrosion of weldments to that of wrought materials. The article discusses the most important methods available to minimize corrosion in weldments.
A. Wahid, D.L. Olson, D.K. Matlock, C.E. Cross, Corrosion of Weldments, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 189–196, https://doi.org/10.31399/asm.tb.wip.t65930189