Steel Heat Treating Fundamentals and Processes
Abstract
Spray quenching refers to a wide variety of quenching processes that involve heat removal facilitated by the impingement of a quenchant medium on a hot metal surface. This article provides information on the basic concepts of spray quenching, and discusses the most commonly used techniques in quench tank agitation to establish uniformity of the quenched part. Common techniques include quenchant stirring, quenchant circulation, and submerged jet/spray mixing. The article also describes the effect of quenching agitation and reviews heat-transfer characteristics of immersion quenching and spray quenching with water.
Spray Quenching, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 245–251, https://doi.org/10.31399/asm.hb.v04a.a0005816
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.