Cold and Cryogenic Treatment of Steel
By
F. Diekman
F. Diekman
Controlled Thermal Processing
Revising author
Search for other works by this author on:
-
Published:2013
Abstract
Cold treating of steel can be used to enhance the transformation of austenite to martensite and improve the stress relief of castings and machined parts. Cryogenic treatment of steel is a distinct process that uses extreme cold to modify the performance of materials. This article explains the practices employed and equipment used in the cold treatment of steel. It also presents the results of using cryogenic treatment to enhance steel properties.
You do not currently have access to this chapter.
Citation
F. Diekman, Cold and Cryogenic Treatment of Steel, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 382–386, https://doi.org/10.31399/asm.hb.v04a.a0005822
Download citation file:
Related Book Content
Hardness and Hardenability of Steels
Steel Heat Treating Fundamentals and Processes
Temper Colors for Steels
Heat Treating of Irons and Steels
Introduction to Cast Iron Heat Treatment
Cast Iron Science and Technology
Austenitizing and Typical Heat Treatment Temperatures for Steels
Heat Treating of Irons and Steels
Acoustical Characterization
Steel Heat Treating Technologies
Quench Factor Characterization of Quenchants for Hardening of Steel
Steel Heat Treating Technologies
Thermoreactive Deposition/Diffusion Process for Surface Hardening of Steels
Steel Heat Treating Fundamentals and Processes
Steel Selection for Hardening
Heat Treating of Irons and Steels
Carburizing
Friction, Lubrication, and Wear Technology
Heat Treatment Problems Associated with Design and Steel Selection
Heat Treating of Irons and Steels