Materials at Low Temperatures
Abstract
This chapter presents basic principles and the theoretical results of heat transport in solids. Thermal conductivity and thermal diffusivity are the principal properties discussed. Discussions are also included on the effects of temperature, magnetic field, and metallurgical variations caused by composition, processing, and heat-treatment differences. Numerous graphs illustrate the qualitative and quantitative effects of these variables. Measurement methods and associated accuracies and pertinent empirical correlations are presented.
Sign in
ASM members
Member Sign InJ. G. Hust, Thermal Conductivity and Thermal Diffusivity, Materials at Low Temperatures, Edited By Richard P. Reed, Alan F. Clark, ASM International, 1983, p 133–161, https://doi.org/10.31399/asm.tb.mlt.t62860133