Failure Analysis of a Misaligned and Unbalanced Flexible Rotor Available to Purchase
-
Published:2019
Abstract
Shaft misalignment and rotor unbalance contribute to the premature failure of many machine components. To understand how these failures occur and quantify the effects, investigators developed a model of a rotating assembly, including a motor, flexible coupling, driveshaft, and bearings. Equations of motion accounting for misalignment and unbalance were then derived using finite elements. A spectral method for resolving these equations was also developed, making it possible to obtain and analyze dynamic system response and identify misalignment and unbalance conditions.
M.A. Hili, T. Fakhfakh, M. Haddar, Failure Analysis of a Misaligned and Unbalanced Flexible Rotor, Handbook of Case Histories in Failure Analysis, Vol 3, Edited By Larry Berardinis, ASM International, 2019, p 695–704, https://doi.org/10.31399/asm.fach.v03.c9001851
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.