Stress-Corrosion Cracking of Stainless Steel Heat Exchanger Tubes in a Fertilizer Plant Available to Purchase
-
Published:1992
Abstract
Several type 304L (UNS S30400) stainless steel seamless tubes in a high-pressure synthesis gas cooler condensing ammonia in a fertilizer plant leaked in an unexpectedly short time. Representative samples of the tubes were subjected to chemical analysis, hardness tests, and optical microscopy examination. The tests revealed that the tubes conformed to specification. Crack morphology indicated stress-corrosion cracking by chlorides present in the cooling water. Use of a duplex stainless steel (for example, UNS S32304 S31803) as a tube material was recommended.
K.E. Perumal, Stress-Corrosion Cracking of Stainless Steel Heat Exchanger Tubes in a Fertilizer Plant, Handbook of Case Histories in Failure Analysis, Vol 1, Edited By Khlefa A. Esaklul, ASM International, 1992, p 126–127, https://doi.org/10.31399/asm.fach.v01.c9001048
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.