Elevated-Temperature Properties of Stainless Steels
-
Published:1990
Abstract
Stainless steels are widely used at elevated temperatures when carbon and low-alloy steels do not provide adequate corrosion resistance and/or sufficient strength at these temperatures. This article deals with the wrought stainless steels used for high temperature applications. It gives some typical compositions of wrought heat-resistant stainless steels, which are grouped into ferritic, martensitic, austenitic, and precipitation-hardening (PH) grades. Quenched and tempered martensitic stainless steels are essentially martensitic and harden when air cooled from the austenitizing temperature. These alloys offer good combinations of mechanical properties. The article focuses on mechanical property considerations and corrosion resistance considerations of stainless steels....
Sign in
ASM members
Member Sign InElevated-Temperature Properties of Stainless Steels, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 930–949, https://doi.org/10.31399/asm.hb.v01.a0001048
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!