Failure of a Laminated-Paper Food Cooking Tray Available to Purchase
-
Published:1993
Abstract
A laminated-paper microwave food tray collapsed with hot food in it. Microscopic examination of the failed tray revealed no structural or material defects. Five additional trays of like construction were also tested to determine the conditions necessary to simulate the permanent deflection of the tray handles that had occurred in the failed tray. Full distortion of the handles was obtained experimentally only by dropping a full hot tray on its end onto the floor. The test results indicated that the tray had slipped from the hand of the user.
David O. Leeser, Failure of a Laminated-Paper Food Cooking Tray, Handbook of Case Histories in Failure Analysis, Vol 2, Edited By Khlefa A. Esaklul, ASM International, 1993, p 480–481, https://doi.org/10.31399/asm.fach.v02.c9001274
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.