Extrusion (Second Edition)
Chapter 6: Machinery and Equipment for Direct and Indirect Hot Extrusion[1]
-
Published:2006
Abstract
The machinery and equipment required for rod and tube extrusion is determined by the specific extrusion process. This chapter provides a detailed description of the design requirements and principles of machinery and equipment for direct and indirect hot extrusion. It then covers the presses and auxiliary equipment for tube extrusion, induction furnaces for billet processing, handling systems for copper and aluminum alloy products, extrusion cooling systems, and age-hardening ovens. Next, the chapter describes the principles and applications of equipment for the production of aluminum and copper billets. Then, it focuses on process control in both direct and indirect hot...
Sign in
ASM members
Member Sign InHorst Groos, Machinery and Equipment for Direct and Indirect Hot Extrusion, Extrusion, 2nd ed., By A.F. Castle;Edited By M. Bauser, G. Sauer, K. Siegert, ASM International, 2006, p 323–416, https://doi.org/10.31399/asm.tb.ex2.t69980323
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field