Abstract
This chapter discusses the types of sensors used in sheet forming operations and the information they provide. It explains how force sensors protect equipment from overloads due to tool wear, friction, and misfeeds, how displacement and proximity sensors help to prevent die crashes, how acoustic emission, ultrasonic, and eddy current sensors detect tool breakage and part defects such as cracks, and how roller ball and optical sensors measure material flow. It also discusses the role of draw-in, wrinkle, oil-monitoring, and vision sensors and explains how material properties can be derived in real time from various sensor outputs.
Deepak Ravindran, Yu-Chih Su, Sensors for Sheet Metal Forming, Sheet Metal Forming: Processes and Applications, Edited By Taylan Altan, A. Erman Tekkaya, ASM International, 2012, p 301–315, https://doi.org/10.31399/asm.tb.smfpa.t53500301
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.