Abstract
Magnetically soft materials are characterized by their low coercivity, an essential requirement for irons and steels selected for any application involving electromagnetic induction cycling. This article provides information on ferromagnetic material properties and how they are affected by impurities, alloying additions, heat treatment, residual stress, and grain size. It also describes classification and testing methods for magnetically soft materials such as high-purity iron, low-carbon steels, silicon steels, iron-aluminum alloys, nickel-iron alloys, iron-cobalt alloys, ferrites, and stainless steels. The article also addresses corrosion resistance and provides insights on the selection of alloys for power generation applications, including motors, generators, and...
Sign in
ASM members
Member Sign InDouglas W. Dietrich, Magnetically Soft Materials, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 761–781, https://doi.org/10.31399/asm.hb.v02.a0001093
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field