Failure Analysis and Prevention (2021 Edition)
X-Ray Diffraction Residual-Stress Measurement in Failure Analysis
-
Published:2021
Abstract
X-ray diffraction (XRD) residual-stress analysis is an essential tool for failure analysis. This article focuses primarily on what the analyst should know about applying XRD residual-stress measurement techniques to failure analysis. Discussions are extended to the description of ways in which XRD can be applied to the characterization of residual stresses in a component or assembly and to the subsequent evaluation of corrective actions that alter the residual-stress state of a component for the purposes of preventing, minimizing, or eradicating the contribution of residual stress to premature failures. The article presents a practical approach to sample selection and specimen...
Sign in
ASM members
Member Sign InJ.A. Pineault, M. Belassel, M.E. Brauss, X-Ray Diffraction Residual-Stress Measurement in Failure Analysis, Failure Analysis and Prevention, Vol 11, 2021 ed., ASM Handbook, Edited By Brett A. Miller, Roch J. Shipley, Ronald J. Parrington, Daniel P. Dennies, ASM International, 2021, p 221–239, https://doi.org/10.31399/asm.hb.v11.a0006768
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.