Abstract
This article describes the coating materials, surface-preparation requirements, and application techniques used to protect underground pipelines. It provides a valuable insight into the types of polymer-based coatings that are both cost-effective and widely accepted in the pipeline industry.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
E. Bud Senkowski, Pipeline Industry Coatings, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 327–339, https://doi.org/10.31399/asm.hb.v05b.a0006038
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
An Example of Blistering Due to Hydrogen Occlusion
ASM Failure Analysis Case Histories: Chemical Processing Equipment
Wax-Based Coating Systems
Protective Organic Coatings
Powder Coatings—Pipelines
Protective Organic Coatings
Polyurethane Coatings
Protective Organic Coatings
Examination of a Blistered and Cracked Natural Gas Line
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Heat Treatment of Cobalt-Base Alloys
Heat Treating of Nonferrous Alloys
Anodic Protection
Corrosion in the Petrochemical Industry (Second Edition)
Marine Cathodic Protection
Corrosion: Environments and Industries
Introduction to Thermal Spray Technology
Thermal Spray Technology
Cathodic Protection
Corrosion in the Petrochemical Industry (Second Edition)