This article discusses the occupational health hazards related to industrial protective coating application and removal. It explains the health hazards associated with coating constituents such as lead, cadmium, chromium, arsenic, silica, and asbestos. The article also discusses hazard evaluation, hazard controls, Occupational Safety and Health Administration standards, and industry consensus standards. It concludes with a description of containment systems to prevent environmental exposures from industrial paint removal projects.
Dan O'Malley, Stanford T. Liang, Worker Health and Environmental Hazards Associated with Coating Application and Removal, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 277–290, https://doi.org/10.31399/asm.hb.v05b.a0006030
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!